42 2740 Special Alloy

Chemical composition%of the ladle analysis of grade42 2740

C(%)Si(%)Mn(%)P(%)S(%)Cr(%)Ni(%)Mo(%)V(%)Cu(%)
0.11-0.190.20-0.500.60-1.000.0350.0351.00-1.500.300.40-0.600.50-0.700.30
42 2740

Mechanical properties of grade42 2740

Proof strength
Rp0.2(MPa)
Tensile strength
Rm(MPa)
Impact energy
KV(J)
Elongation at fracture
A(%)
Reduction in cross section on fracture
Z(%)
As-Heat-Treated Condition Brinell hardness(HBW)
619(≥) 369(≥) 21 21 32 Solution and Aging,Annealing,Ausaging,Q+T,etc 214

Physical properties of grade 42 2740

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J/kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
245(≥) 189(≥) 33 12 43 Solution and Aging,Annealing,Ausaging,Q+T,etc 113
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0)N/mm2
Creep rupture strength
(10000h)
(Rp1,0)N/mm2
935 553 728

42 2740 Range of products

Product type Products Dimension Processes Deliver Status
Plates/Sheets Plates/Sheets 0.08-200mm(T)*W*L Forging,hot rolling and cold rolling Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Steel Bar Round Bar,Flat Bar,Square Bar Φ8-1200mm*L Forging,hot rolling and cold rolling,Cast Black,Rough Turning,Shot Blasting,
Coil/Strip Steel Coil/Steel Strip 0.03-16.0x1200mm Cold-Rolled&Hot-Rolled Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Pipes/Tubes Seamless Pipes/Tubes,Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion,Cold Drawn,Welded Annealed,Solution and Aging,Q+T,ACID-WASHED

42 2740 Steel Stock

Steel grade Dimension Shape Unit Quantity Delivery state Query
SA-437 Grade B4B/SUS 616 /422 Forged Bar Dia.160xL Round Bar Kgs 2120 Forged+QT Enquiry
Stainless Steel 422 / Alloy 422 AMS 5655 UNS S42200/616/B4B Round Bar Stock Select 0 Select Enquiry