Cold rolled stainless steel sheets and plates

Chemical composition(wt.%) of 4Cr13 grade: to GB/T 1220 (1992)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.36 0.45
Si - 0.60
Mn - 0.80
P - 0.035
S - 0.030
Ni - 0.60
Cr 12.00 14.00

4Cr13 - Detail

4Cr13

Mechanical properties of grade 4Cr13 GB/T 1220 (1992)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
427 (≥) 994 (≥) 21 21 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 243

Physical properties of grade 4Cr13 GB/T 1220 (1992)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
657 (≥) 745 (≥) 21 24 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 441
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
748 698 482