664.3 Special Alloy

Chemical composition%of the ladle analysis of grade664.3

C(%)Si(%)Mn(%)Cr(%)
3.00-4.500.30-0.700.30-0.7026.0-31.0
664.3

Mechanical properties of grade664.3

Proof strength
Rp0.2(MPa)
Tensile strength
Rm(MPa)
Impact energy
KV(J)
Elongation at fracture
A(%)
Reduction in cross section on fracture
Z(%)
As-Heat-Treated Condition Brinell hardness(HBW)
598(≥) 853(≥) 22 22 34 Solution and Aging,Annealing,Ausaging,Q+T,etc 124

Physical properties of grade 664.3

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J/kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
994(≥) 211(≥) 43 12 12 Solution and Aging,Annealing,Ausaging,Q+T,etc 144
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0)N/mm2
Creep rupture strength
(10000h)
(Rp1,0)N/mm2
172 636 416

664.3 Range of products

Product type Products Dimension Processes Deliver Status
Plates/Sheets Plates/Sheets 0.08-200mm(T)*W*L Forging,hot rolling and cold rolling Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Steel Bar Round Bar,Flat Bar,Square Bar Φ8-1200mm*L Forging,hot rolling and cold rolling,Cast Black,Rough Turning,Shot Blasting,
Coil/Strip Steel Coil/Steel Strip 0.03-16.0x1200mm Cold-Rolled&Hot-Rolled Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Pipes/Tubes Seamless Pipes/Tubes,Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion,Cold Drawn,Welded Annealed,Solution and Aging,Q+T,ACID-WASHED

664.3 Steel Stock

Steel grade Dimension Shape Unit Quantity Delivery state Query
17-4PH Coil Stock 0.08*200mm Coil or Strip Kgs 1623 Cold-Rolled+Annealed Enquiry
17-4PH Round Bar Φ5-300mm*L Round Bar Kgs 46958 Hot-Rolled+Annealed+black Enquiry
17-4PH plate 8-45*1200*3000mm Plate or Sheet Tons 4.9 Hot-Rolled+Annealed+black Enquiry
Cr12MoV 12-160(T)*310-610(W)*L Plate or Sheet Tons 12.38 Hot-Rolled+Annealed+black Enquiry
1.2601 12-160(T)*310-610(W)*L Plate or Sheet Tons 11.22 Hot-Rolled+Annealed+black Enquiry
IncoloyA-286 / GH 2132 Stock Φ8-65mm*L Round Bar Kgs 489 Hot-Rolled+Annealed+black Enquiry
17-7PH / 631 Coil & Strip, Sheet Stock 0.3-3.0*10-180mm Coil or Strip Kgs 1236.22 Cold-Rolled+Annealed Enquiry
X22CrMoV12-1 / 1.4923 Φ17mm Round Bar Kgs 300 Hot-Rolled+Annealed+black Enquiry
1.2083 Forged Plate T:105-185mm*W:510*L Plate or Sheet Tons 26 Forged+QT Enquiry
X22CrMoV12-1 / 1.4923 Φ30mm Round Bar Kgs 300 Hot-Rolled+Annealed+black Enquiry
A387 F5 & Grade 5 sheet Coil strip 0.5mmx200mmxC Coil or Strip Tons 3 Cold-Rolled+Annealed Enquiry
A387 F5 & Grade 5 Hot Coil stock Select Tons 3 Hot-Rolled+Annealed+black Enquiry
T45Cr5Si3 Round Bar Dia.40mm Round Bar Kgs 500 Hot-Rolled+Annealed+black Enquiry
UNS K30960(VIM+ESR) Bright Round Bar Dia.22mm Round Bar Kgs 50 Hot-Rolled+Annealed+black Enquiry
H13 Tool Steel 50x710xL Flat or Square bar PCS 4 Forged+Annealed+black Enquiry
1.2344(H13/X40CrMoV5-1/Z40CDV5) Stock List Dia.182mm - Dia.510mm Round Bar Tons 120 Forged+Annealed+black Enquiry
1.2344 ESR Round Bar Stock List(2019-9-3) Select 0 Select Enquiry
1.2343 ESR Stock list(2019-09-03) Select 0 Select Enquiry
1.2367 ESR Forged Round Bar stock(2019-09-03) Select 0 Select Enquiry
1.2379 ESR Round Bar Stock(2019-09-03) Select 0 Select Enquiry