7Cr17 Stainless Steels to GB/T 1220 (1992)

7Cr17 - Specification & Application

  • GB/T 1220 (1992) - Stainless steel bars
  • GB/T 3280 (2007) - Cold rolled stainless steel sheets and plates
  • GB/T 4237 (1992) - Hot rolled stainless steel sheets and plates
  • GB/T 4239 (1991) - Cold rolled stainless steel and heat resisting steel strips
  • GB/T 4356 (2002) - Stainless steel wire rods

Stainless steel bars

Chemical composition(wt.%) of 7Cr17 grade: to GB/T 1220 (1992)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.60 0.75
Si - 1.00
Mn - 1.00
Ni - 0.60
Cr 16.00 18.00
Mo - 0.75

7Cr17 - Detail

7Cr17

Mechanical properties of grade 7Cr17 GB/T 1220 (1992)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
888 (≥) 417 (≥) 21 14 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 432

Physical properties of grade 7Cr17 GB/T 1220 (1992)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
266 (≥) 892 (≥) 42 34 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 323
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
615 214 478

Equivalent Grade

Equivalent Products

We can customize the production of 7Cr17 grade, contact us for the best solution.