A 1014 N07718 Superalloys to A 1014/A 1014M (2010)

A 1014 N07718 - Specification & Application

  • A 1014/A 1014M (2010) - Standard Specification for Precipitation-Hardening Bolting (UNS N07718) for High Temperature Service

Standard Specification for Precipitation-Hardening Bolting (UNS N07718) for High Temperature Service

Chemical composition(wt.%) of A 1014 N07718 grade: to A 1014/A 1014M (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Cr 17.0 21.0
Mo 2.80 3.30
Ni 50.0 55.0
Al 0.20 0.60
Nb 4.75 5.50
Fe - Bal
Si - 0.35
Mn - 0.35
P - 0.015
S - 0.015
B - 0.006

A 1014 N07718 - Detail

A 1014 N07718

Mechanical properties of grade A 1014 N07718 A 1014/A 1014M (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
829 (≥) 391 (≥) 32 23 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 142

Physical properties of grade A 1014 N07718 A 1014/A 1014M (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
736 (≥) 226 (≥) 21 13 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 144
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
442 992 329