A 216 Grade WCB Stainless Steels to A 216/A 216M (2012)

A 216 Grade WCB - Specification & Application

  • A 216/A 216M (2012) - Steel Castings, Carbon, Suitable for Fusion Welding, for High-Temperature Service

Steel Castings, Carbon, Suitable for Fusion Welding, for High-Temperature Service

Chemical composition(wt.%) of A 216 Grade WCB grade: to A 216/A 216M (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn 7.50 9.00
P - -
S - -
Ni 5.00 7.00
Cr 17.50 22.00
Al - -
Cu - -
Ti - -
Fe - -
N 0.25 0.50
Mo 2.00 3.00

A 216 Grade WCB - Detail

Steel Castings, Carbon, Suitable for Fusion Welding, for High-Temperature Service

Mechanical properties of grade A 216 Grade WCB A 216/A 216M (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
177 (≥) 666 (≥) 23 13 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 341

Physical properties of grade A 216 Grade WCB A 216/A 216M (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
657 (≥) 937 (≥) 42 41 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 111
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
124 196 362
We can customize the production of A 216 Grade WCB grade, contact us for the best solution.