A 240 S44627 Stainless Steels to A 240/A 240M (2012)

A 240 S44627 - Specification & Application

  • A 240/A 240M (2012) - Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications

Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications

Chemical composition(wt.%) of A 240 S44627 grade: to A 240/A 240M (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.01
Mn - 0.40
Si - 0.40
P - 0.02
S - 0.02
Cr 25.00 27.00
Ni - 0.50
Mo 0.75 1.50
N - 0.015
Cu - 0.020
Nb 0.05 0.20

A 240 S44627 - Detail

Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications

Mechanical properties of grade A 240 S44627 A 240/A 240M (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
236 (≥) 725 (≥) 11 14 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 131

Physical properties of grade A 240 S44627 A 240/A 240M (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
765 (≥) 695 (≥) 44 44 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 344
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
958 368 953

Equivalent Products

We can customize the production of A 240 S44627 grade, contact us for the best solution.