A 501 Grade B Stainless Steels to A 501 (2007)

A 501 Grade B - Specification & Application

  • A 501 (2007) - Hot-Formed Welded and Seamless Carbon Steel Structural Tubing

Hot-Formed Welded and Seamless Carbon Steel Structural Tubing

Chemical composition(wt.%) of A 501 Grade B grade: to A 501 (2007)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Mn 0.30 0.60
Si 0.50 1.00
P - 0.03
S - 0.03
Cr 8.00 10.00
Ni - -
Mo 0.90 1.10

A 501 Grade B - Detail

Hot-Formed Welded and Seamless Carbon Steel Structural Tubing

Mechanical properties of grade A 501 Grade B A 501 (2007)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
268 (≥) 732 (≥) 24 21 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 222

Physical properties of grade A 501 Grade B A 501 (2007)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
288 (≥) 989 (≥) 31 22 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 434
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
995 698 779

Equivalent Products

We can customize the production of A 501 Grade B grade, contact us for the best solution.