A 554 S43400 Stainless Steels to A 554 (2011)

A 554 S43400 - Specification & Application

  • A 554 (2011) - Welded Stainless Steel Mechanical Tubing

Welded Stainless Steel Mechanical Tubing

Chemical composition(wt.%) of A 554 S43400 grade: to A 554 (2011)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.12
Mn - 1.00
Si - 1.00
P - 0.04
S - 0.03
Cr 16.00 18.00
Ni - -
Mo 0.75 1.25

A 554 S43400 - Detail

Welded Stainless Steel Mechanical Tubing

Mechanical properties of grade A 554 S43400 A 554 (2011)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
566 (≥) 365 (≥) 41 11 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 422

Physical properties of grade A 554 S43400 A 554 (2011)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
888 (≥) 284 (≥) 23 21 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 113
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
285 559 319

Equivalent Products

We can customize the production of A 554 S43400 grade, contact us for the best solution.
sales@specificsteel.com