A 581 S41610 Stainless Steels to A 581/A 581M (2009)

A 581 S41610 - Specification & Application

  • A 581/A 581M (2009) - Free-Machining Stainless Steel Wire and Wire Rods

Free-Machining Stainless Steel Wire and Wire Rods

Chemical composition(wt.%) of A 581 S41610 grade: to A 581/A 581M (2009)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.15 -
Mn 1.50 2.50
Si - 1.00
P - 0.06
S - 0.15
Cr 12.00 14.00
Ni - -
Mo - 0.60

A 581 S41610 - Detail

Free-Machining Stainless Steel Wire and Wire Rods

Mechanical properties of grade A 581 S41610 A 581/A 581M (2009)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
542 (≥) 237 (≥) 32 14 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 111

Physical properties of grade A 581 S41610 A 581/A 581M (2009)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
893 (≥) 543 (≥) 32 42 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 444
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
597 211 415
We can customize the production of A 581 S41610 grade, contact us for the best solution.