A 959 S33228 Stainless Steels to A 959 (2011)

A 959 S33228 - Specification & Application

  • A 959 (2011) - Standard Guide for Specifying Harmonized Standard Grade Compositions for Wrought Stainless Steels

Standard Guide for Specifying Harmonized Standard Grade Compositions for Wrought Stainless Steels

Chemical composition(wt.%) of A 959 S33228 grade: to A 959 (2011)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04 0.08
Mn - 1.00
Si - 0.30
P - 0.02
S - 0.015
Cr 26.0 28.0
Ni 31.0 33.0
Ce 0.05 0.10
Nb 0.10 1.00
Al - 0.025

A 959 S33228 - Detail

Standard Guide for Specifying Harmonized Standard Grade Compositions for Wrought Stainless Steels

Mechanical properties of grade A 959 S33228 A 959 (2011)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
482 (≥) 672 (≥) 32 41 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 142

Physical properties of grade A 959 S33228 A 959 (2011)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
429 (≥) 447 (≥) 14 13 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 422
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
572 989 591