ASTM 50Cr-50Ni-Nb Superalloys

ASTM 50Cr-50Ni-Nb - Specification & Application

Standard Specification for Castings, Chromium-Nickel Alloy

Chemical composition(wt.%) of ASTM 50Cr-50Ni-Nb grade:

Elements Min.(≥) Max.(≤) Similar Remarks

ASTM 50Cr-50Ni-Nb - Detail

Standard Specification for Castings, Chromium-Nickel Alloy
This standard is issued under the fixed designation A 560/A 560M; the number immediately following the designation indicates the year of original adoption or, in the case of revision, the year of last revision. A number in parentheses indicates the year of last reapproval. A superscript epsilon (e) indicates an editorial change since the last revision or reapproval

Mechanical properties of grade ASTM 50Cr-50Ni-Nb

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
534 (≥) 996 (≥) 41 41 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 411

Physical properties of grade ASTM 50Cr-50Ni-Nb

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
687 (≥) 935 (≥) 12 34 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 441
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
612 178 236