B 435 N12160 Stainless Steels to B 435 (2011)

B 435 N12160 - Specification & Application

  • B 435 (2011) - UNS N06002, UNS N06230, UNS N12160, and UNS R30556 Plate, Sheet, and Strip

UNS N06002, UNS N06230, UNS N12160, and UNS R30556 Plate, Sheet, and Strip

Chemical composition(wt.%) of B 435 N12160 grade: to B 435 (2011)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn 7.50 9.00
P - -
S - -
Ni 5.00 7.00
Cr 17.50 22.00
Al - -
Cu - -
Ti - -
Fe - -
N 0.25 0.50
Mo 2.00 3.00

B 435 N12160 - Detail

UNS N06002, UNS N06230, UNS N12160, and UNS R30556 Plate, Sheet, and Strip

Mechanical properties of grade B 435 N12160 B 435 (2011)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
511 (≥) 293 (≥) 22 34 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 342

Physical properties of grade B 435 N12160 B 435 (2011)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
286 (≥) 656 (≥) 24 32 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 231
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
518 798 359