Precipitation-Hardening Nickel Alloy (UNS N07718) Plate, Sheet, and Strip for High-Temperature Service
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.03 | ||
Cr | 17.0 | 21.0 | ||
Mo | 2.80 | 3.30 | ||
Ni | 50.0 | 55.0 | ||
Al | 0.20 | 0.60 | ||
Nb | 4.75 | 5.50 | ||
Fe | - | Bal | ||
Si | - | 0.35 | ||
Mn | - | 0.35 | ||
P | - | 0.015 | ||
S | - | 0.015 | ||
B | - | 0.006 |
B 637 N07718
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
555 (≥) | 362 (≥) | 44 | 44 | 41 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 342 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
236 (≥) | 345 (≥) | 21 | 42 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 414 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
728 | 673 | 496 |
We can customize the production of B 670 N07718 grade, contact us for the best solution.
–sales@specificsteel.com