C105W2 Tool Die Steels

C105W2 - Specification & Application

High carbon steel

Chemical composition(wt.%) of C105W2 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 1.00 1.10
Si 0.10 0.30
Mn 0.10 0.25
P - 0.030
S - 0.030

C105W2 - Detail

High carbon steel

Mechanical properties of grade C105W2

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
294 (≥) 629 (≥) 33 13 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 433

Physical properties of grade C105W2

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
242 (≥) 522 (≥) 42 43 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 124
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
886 973 948

Equivalent Grade

Equivalent Products

We can customize the production of C105W2 grade, contact us for the best solution.