Custom 450 Stainless Steels to SAE AMS 5863E (2009)

Custom 450 - Specification & Application

  • SAE AMS 5863E (2009) - Steel, Corrosion Resistant, Sheet, Strip, and Plate 15Cr - 6.5Ni - 0.75Mo - 0.60Cb - 1.5Cu Solution Heat Treated, Precipitation Hardenable

Steel, Corrosion Resistant, Sheet, Strip, and Plate 15Cr - 6.5Ni - 0.75Mo - 0.60Cb - 1.5Cu Solution Heat Treated, Precipitation Hardenable

Chemical composition(wt.%) of Custom 450 grade: to SAE AMS 5863E (2009)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.05
Si - 1.00
Mn - 1.00
P - -
S - -
Ni 5.00 7.00
Cr 14.00 16.00
Al - -
Cu 1.25 1.75
Ti - -
Fe - -
Mo 0.50 1.00
Co - -
Nb - -

Custom 450 - Detail

Steel, Corrosion Resistant, Sheet, Strip, and Plate 15Cr - 6.5Ni - 0.75Mo - 0.60Cb - 1.5Cu Solution Heat Treated, Precipitation Hardenable

Mechanical properties of grade Custom 450 SAE AMS 5863E (2009)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
571 (≥) 186 (≥) 43 32 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 121

Physical properties of grade Custom 450 SAE AMS 5863E (2009)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
192 (≥) 536 (≥) 34 11 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 444
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
934 759 959

Equivalent Products

We can customize the production of Custom 450 grade, contact us for the best solution.
sales@specificsteel.com