Custom 455 Stainless Steels to SAE AMS 5672C (2000)

Custom 455 - Specification & Application

  • SAE AMS 5672C (2000) - Steel Wire, Corrosion Resistant 11.8Cr - 8.5Ni - 0.30(Cb + Ta) - 1.1Ti - 2.0Cu Precipitation Hardenable, Spring Temper

Steel Wire, Corrosion Resistant 11.8Cr - 8.5Ni - 0.30(Cb + Ta) - 1.1Ti - 2.0Cu Precipitation Hardenable, Spring Temper

Chemical composition(wt.%) of Custom 455 grade: to SAE AMS 5672C (2000)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.02
Si - -
Mn - -
P - -
S - -
Ni - 8.50
Cr - 12.00
Al - -
Cu - 2.00
Ti - 1.15
Fe - remaining
Mo - -
Co - -
Nb - 0.38
B - 0.003

Custom 455 - Detail

Steel Wire, Corrosion Resistant 11.8Cr - 8.5Ni - 0.30(Cb + Ta) - 1.1Ti - 2.0Cu Precipitation Hardenable, Spring Temper

Mechanical properties of grade Custom 455 SAE AMS 5672C (2000)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
236 (≥) 271 (≥) 23 42 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 414

Physical properties of grade Custom 455 SAE AMS 5672C (2000)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
226 (≥) 857 (≥) 33 21 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 132
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
416 923 437

Equivalent Products

We can customize the production of Custom 455 grade, contact us for the best solution.
sales@specificsteel.com