D6AC Stainless Steels to SAE AMS-S-8949B (1998)

D6AC - Specification & Application

  • SAE AMS-S-8949B (1998) - Steel Bars, Plates, Sheets, Billets, and Reforging Stock Type D6AC

Steel Bars, Plates, Sheets, Billets, and Reforging Stock Type D6AC

Chemical composition(wt.%) of D6AC grade: to SAE AMS-S-8949B (1998)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.47
Si - 0.22
Mn - 0.75
P - -
S - -
Ni - 0.55
Cr - 1.05
Al - -
Cu - -
Ti - -
Fe - remaining
Mo - 1.00
Co - -
V - 0.10

D6AC - Detail

Steel Bars, Plates, Sheets, Billets, and Reforging Stock Type D6AC

Mechanical properties of grade D6AC SAE AMS-S-8949B (1998)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
982 (≥) 664 (≥) 14 22 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 111

Physical properties of grade D6AC SAE AMS-S-8949B (1998)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
436 (≥) 522 (≥) 21 13 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 434
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
521 877 197