DNVGL VL NV D36 Structural Steel

DNVGL VL NV D36 - Specification & Application

High Strength Structural Steel Plate

Chemical composition(wt.%) of DNVGL VL NV D36 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.18
Si - 0.50
Mn 0.90 1.60
P - 0.035
S - 0.035
Cr - 0.20
Mo - 0.08
Ni - 0.40
Al - 0.020
Cu - 0.35
Nb 0.02 0.05
Ti 0.007 0.05
V 0.05 0.10

DNVGL VL NV D36 - Detail

DNVGL VL NV D36 High Strength Structural Steel Plate

Mechanical properties of grade DNVGL VL NV D36

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
969 (≥) 681 (≥) 14 23 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 242

Physical properties of grade DNVGL VL NV D36

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
662 (≥) 177 (≥) 31 13 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 321
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
614 971 856