E-Z6NCT25 Air 9160/C Aviation and Aero Steel to AIR 9160 C

E-Z6NCT25 Air 9160/C - Specification & Application

  • AIR 9160 C - wrought steels used in aeronautical constructions

wrought steels used in aeronautical constructions

Chemical composition(wt.%) of E-Z6NCT25 Air 9160/C grade: to AIR 9160 C

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si 0.40 1.00
Mn 1.00 2.00
P - 0.030
S - 0.015
Cr 13.50 16.00
Ni 24.00 27.00
Mo 1.00 1.50
V 0.10 0.50
Al - 0.35
Ti 1.90 2.300
B 0.001 0.010

E-Z6NCT25 Air 9160/C - Detail

E-Z6NCT25 Air 9160C wrought steels used in aeronautical constructions

Mechanical properties of grade E-Z6NCT25 Air 9160/C AIR 9160 C

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
595 (≥) 829 (≥) 13 34 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 314

Physical properties of grade E-Z6NCT25 Air 9160/C AIR 9160 C

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
253 (≥) 739 (≥) 12 22 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 212
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
662 873 159

Equivalent Grade

Equivalent Products

We can customize the production of E-Z6NCT25 Air 9160/C grade, contact us for the best solution.