EH11K Stainless Steels to A5.17/A5.17M

EH11K - Specification & Application

  • A5.17/A5.17M - Carbon Steel Electrodes and Fluxes for Submerged Arc Welding

Carbon Steel Electrodes and Fluxes for Submerged Arc Welding

Chemical composition(wt.%) of EH11K grade: to A5.17/A5.17M

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.40
Si - 0.90
Mn - 0.30
P - -
S - -
Ni - -
Cr - 5.00
Al - -
Cu - -
Ti - -
Fe - remaining
Mo - 1.30
Co - -
V - 0.50

EH11K - Detail

Carbon Steel Electrodes and Fluxes for Submerged Arc Welding

Mechanical properties of grade EH11K A5.17/A5.17M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
811 (≥) 838 (≥) 43 42 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 341

Physical properties of grade EH11K A5.17/A5.17M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
268 (≥) 287 (≥) 13 14 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 324
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
991 763 388

Equivalent Products

We can customize the production of EH11K grade, contact us for the best solution.