Standard Specification for Wrought Titanium-3Aluminum-2.5Vanadium Alloy Seamless Tubing for Surgical Implant Applications (UNS R56320)
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.05 | ||
Si | - | 0.20 | ||
Mn | - | 0.50 | ||
P | - | - | ||
S | - | - | ||
Ni | - | remaining | ||
Cr | 15.00 | 17.00 | ||
Al | 4.00 | 5.00 | ||
Cu | - | - | ||
Ti | - | 0.50 | ||
Fe | 2.00 | 4.00 | ||
N | - | - | ||
Mo | - | 0.50 | ||
B | - | 0.006 | ||
Zr | - | 0.05 |
Standard Specification for Wrought Titanium-3Aluminum-2.5Vanadium Alloy Seamless Tubing for Surgical Implant Applications (UNS R56320)
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
323 (≥) | 521 (≥) | 44 | 12 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 443 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
568 (≥) | 112 (≥) | 41 | 12 | 43 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 222 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
341 | 277 | 723 |
We can customize the production of F2146 R56320 grade, contact us for the best solution.