Fe-Ni29Co-17 Stainless Steels to NF A 54-301

Fe-Ni29Co-17 - Specification & Application

  • NF A 54-301 - Nickel and nickel alloys. Iron-nickel alloys with particular dilatability

Nickel and nickel alloys. Iron-nickel alloys with particular dilatability

Chemical composition(wt.%) of Fe-Ni29Co-17 grade: to NF A 54-301

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.02
Si - 0.20
Mn - 0.25
P - 0.030
S - 0.030
Cr - -
Ni - 29.00
Mo - -
Fe - remaining(54.00)
Co - 17.00

Fe-Ni29Co-17 - Detail

Nickel and nickel alloys. Iron-nickel alloys with particular dilatability

Mechanical properties of grade Fe-Ni29Co-17 NF A 54-301

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
223 (≥) 871 (≥) 34 21 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 313

Physical properties of grade Fe-Ni29Co-17 NF A 54-301

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
913 (≥) 899 (≥) 23 13 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 223
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
489 282 174

Equivalent Products

We can customize the production of Fe-Ni29Co-17 grade, contact us for the best solution.