GH1014 Superalloys

GH1014 - Specification & Application

Iron-based superalloy

Chemical composition(wt.%) of GH1014 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Cr 19.0 22.0
Mo 1.5 2.5
Ni 28.0 34.0
W 7.5 9.5
Nb 0.8 1.3
B - 0.01
Fe - Remainder
Mn - 1.5
Si - 0.6
Ce - 0.05
N 0.15 0.25

GH1014 - Detail

GH1014

Mechanical properties of grade GH1014

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
737 (≥) 489 (≥) 32 31 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 221

Physical properties of grade GH1014

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
323 (≥) 668 (≥) 43 24 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 422
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
174 166 312

Equivalent Grade

Equivalent Products

We can customize the production of GH1014 grade, contact us for the best solution.