GH1035 Stainless Steels to GB/T 14992 (2005)

GH1035 - Specification & Application

  • GB/T 14992 (2005) - Classification and designation for superalloys and high temperature intermetallic materials
  • GB/T 14995 (2010) - Hot-rolled superalloy sheets
  • GB/T 14996 (2010) - Cold-Rolled heat-resisting superalloy sheets

Classification and designation for superalloys and high temperature intermetallic materials

Chemical composition(wt.%) of GH1035 grade: to GB/T 14992 (2005)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.06 0.12
Cr 20.0 23.0
Ni 35.0 40.0
W 2.50 3.50
Al - 0.50
Nb 1.20 1.70
Ti 0.70 1.20
Si - 0.80
Mn - 0.70
P - 0.030
S - 0.020
Ce - 0.05

GH1035 - Detail

Mechanical properties of grade GH1035 GB/T 14992 (2005)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
549 (≥) 639 (≥) 12 32 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 323

Physical properties of grade GH1035 GB/T 14992 (2005)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
317 (≥) 468 (≥) 34 13 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 424
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
574 856 429

Equivalent Grade

Equivalent Products