GH1138 Superalloys

GH1138 - Specification & Application

Iron-based superalloy

Chemical composition(wt.%) of GH1138 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.10
Cr 18.0 22.0
Mo 2.0 2.6
Ni 35.0 40.0
W 4.5 5.2
Al - 0.5
Nb 1.0 1.7
B - 0.008
Fe - Remainder
Mn 1.0 2.0
Si - 0.8
Ce - 0.05
N 0.10 0.25
Zr - 0.05

GH1138 - Detail

GH1138

Mechanical properties of grade GH1138

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
624 (≥) 662 (≥) 12 12 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 243

Physical properties of grade GH1138

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
918 (≥) 347 (≥) 43 42 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 134
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
775 845 871

Equivalent Grade

Equivalent Products

We can customize the production of GH1138 grade, contact us for the best solution.