GH2036 Stainless Steels to GB/T 14992 (2005)

GH2036 - Specification & Application

  • GB/T 14992 (2005) - Classification and designation for superalloys and high temperature intermetallic materials
  • GB/T 14994 (2008) - Cold brawn heat-resisting superalloy bars
  • GB/T 14997 (1994) - Forged heat-resisting superalloy disks
  • GB/T 14998 (1994) - Heat-resisting superalloy blanks for forged rings

Classification and designation for superalloys and high temperature intermetallic materials

Chemical composition(wt.%) of GH2036 grade: to GB/T 14992 (2005)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.34 0.40
Cr 11.5 13.5
Mo 1.10 1.40
Ni 7.00 9.00
Nb 0.25 0.55
Ti - 0.12
Si 0.30 0.80
Mn 7.50 9.50
P - 0.035
S - 0.030
V 1.25 1.55

GH2036 - Detail

GH2036

Mechanical properties of grade GH2036 GB/T 14992 (2005)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
978 (≥) 669 (≥) 32 42 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 241

Physical properties of grade GH2036 GB/T 14992 (2005)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
462 (≥) 432 (≥) 21 44 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 143
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
548 379 497

Equivalent Grade

Equivalent Products

We can customize the production of GH2036 grade, contact us for the best solution.