Classification and designation for superalloys and high temperature intermetallic materials

Chemical composition(wt.%) of GH3044 grade: to GB/T 14992 (2005)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.10
Cr 23.5 26.5
Mo - 1.50
Ni - Remainder
W 13.0 16.0
Al - 0.50
Ti 0.30 0.70
Fe - 4.0
Si - 0.80
Mn - 0.50
P - 0.013
S - 0.013

GH3044 - Detail

GH3044

Mechanical properties of grade GH3044 GB/T 14992 (2005)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
977 (≥) 436 (≥) 13 24 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 223

Physical properties of grade GH3044 GB/T 14992 (2005)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
497 (≥) 961 (≥) 13 23 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 222
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
621 961 694

Equivalent Grade

Equivalent Products

We can customize the production of GH3044 grade, contact us for the best solution.