GH3170 Superalloys

GH3170 - Specification & Application

Iron-based superalloy

Chemical composition(wt.%) of GH3170 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.06
Cr 18.0 22.0
Ni - Remainder
Co 15.0 22.0
W 18.0 21.0
Al - 0.5
B - 0.005
Zr 0.1 0.2
La 0.1 0.3

GH3170 - Detail

GH3170

Mechanical properties of grade GH3170

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
813 (≥) 675 (≥) 44 32 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 434

Physical properties of grade GH3170

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
911 (≥) 455 (≥) 33 12 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 311
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
363 835 241

Equivalent Grade

Equivalent Products

We can customize the production of GH3170 grade, contact us for the best solution.