GH3333 Superalloys

GH3333 - Specification & Application

Iron-based superalloy

Chemical composition(wt.%) of GH3333 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Cr 24.0 27.0
Mo 2.5 4.0
Ni 44.0 47.0
Co 2.5 4.0
W 2.5 4.0
Al - 0.2
Nb - 0.2
Ti - 0.2
B - 0.006
Fe - Remainder

GH3333 - Detail

GH3333

Mechanical properties of grade GH3333

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
333 (≥) 385 (≥) 12 31 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 322

Physical properties of grade GH3333

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
993 (≥) 883 (≥) 43 11 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 322
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
364 288 587

Equivalent Grade

Equivalent Products