GH4141 Superalloys

GH4141 - Specification & Application

Iron-based superalloy

Chemical composition(wt.%) of GH4141 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.06 0.12
Cr 18.0 20.0
Mo 9.0 10.5
Ni - Remainder
Co 10.0 12.0
Al 1.4 2.0
Nb 2.5 3.9
Ti 2.9 3.5
B 0.003 0.01
Fe - 0.5

GH4141 - Detail

GH4141

Mechanical properties of grade GH4141

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
442 (≥) 999 (≥) 21 11 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 424

Physical properties of grade GH4141

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
886 (≥) 935 (≥) 13 41 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 444
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
127 919 615

Equivalent Grade

Equivalent Products

We can customize the production of GH4141 grade, contact us for the best solution.