H41 Tool Die Steels

H41 - Specification & Application

Hot-Work Tool Steel

Chemical composition(wt.%) of H41 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.60 0.75
Si 0.20 0.45
Mn 0.15 0.40
P - 0.030
S - 0.030
Cr 3.50 4.00
Mo 8.20 9.20
V 1.00 1.30
W 1.40 2.10
Ni+Cu - 0.75

H41 - Detail

Hot-Work Tool Steel

Mechanical properties of grade H41

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
755 (≥) 493 (≥) 34 43 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 442

Physical properties of grade H41

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
224 (≥) 276 (≥) 21 31 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 312
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
254 592 918

Equivalent Products

We can customize the production of H41 grade, contact us for the best solution.
sales@specificsteel.com