HEV7 Stainless Steels

HEV7 - Specification & Application

Steel for exhaust valves

Chemical composition(wt.%) of HEV7 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 0.70
Mn - 1.50
P - -
S - -
Cr - 14.75
Ni - 26.0
Mo - 1.25

HEV7 - Detail

Steel for exhaust valves

Mechanical properties of grade HEV7

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
773 (≥) 464 (≥) 13 23 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 334

Physical properties of grade HEV7

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
441 (≥) 511 (≥) 44 13 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 133
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
824 848 358