HP 9-4-20 Stainless Steels to SAE AMS 6523G (2011)

HP 9-4-20 - Specification & Application

  • SAE AMS 6523G (2011) - Steel, Sheet, Strip, and Plate 0.75Cr - 9.0Ni - 4.5Co - 1.0Mo - 0.09V (0.17 - 0.23C) Vacuum Consumable Electrode Melted, Annealed

Steel, Sheet, Strip, and Plate 0.75Cr - 9.0Ni - 4.5Co - 1.0Mo - 0.09V (0.17 - 0.23C) Vacuum Consumable Electrode Melted, Annealed

Chemical composition(wt.%) of HP 9-4-20 grade: to SAE AMS 6523G (2011)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.17 0.23
Si - 0.10
Mn - 0.20
Ni - 0.65
Cr - 0.40
Al 4.25 4.75
Cu - -
Ti - -
Fe - -
Mo - 0.85
Co 8.50 9.50
V 0.06 0.12
P - 0.01
S - 0.01
W 0.90 1.10

HP 9-4-20 - Detail

Steel, Sheet, Strip, and Plate 0.75Cr - 9.0Ni - 4.5Co - 1.0Mo - 0.09V (0.17 - 0.23C) Vacuum Consumable Electrode Melted, Annealed

Mechanical properties of grade HP 9-4-20 SAE AMS 6523G (2011)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
692 (≥) 614 (≥) 31 21 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 313

Physical properties of grade HP 9-4-20 SAE AMS 6523G (2011)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
869 (≥) 866 (≥) 32 32 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 212
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
759 666 726

Equivalent Products

We can customize the production of HP 9-4-20 grade, contact us for the best solution.