ISO 11 Special Alloy

Chemical composition%of the ladle analysis of gradeISO 11

C(%)Si(%)Mn(%)P(%)S(%)Cr(%)Ni(%)N(%)
Max 0.070Max 1.00Max 2.00Max 0.045Max 0.03017.0-19.58.00-10.5Max 0.11
ISO standard thermal deformation of stainless steel

Mechanical properties of gradeISO 11

Proof strength
Rp0.2(MPa)
Tensile strength
Rm(MPa)
Impact energy
KV(J)
Elongation at fracture
A(%)
Reduction in cross section on fracture
Z(%)
As-Heat-Treated Condition Brinell hardness(HBW)
359(≥) 281(≥) 34 22 43 Solution and Aging,Annealing,Ausaging,Q+T,etc 133

Physical properties of grade ISO 11

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J/kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
619(≥) 469(≥) 21 32 24 Solution and Aging,Annealing,Ausaging,Q+T,etc 321
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0)N/mm2
Creep rupture strength
(10000h)
(Rp1,0)N/mm2
918 598 993

ISO 11 Range of products

Product type Products Dimension Processes Deliver Status
Plates/Sheets Plates/Sheets 0.08-200mm(T)*W*L Forging,hot rolling and cold rolling Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Steel Bar Round Bar,Flat Bar,Square Bar Φ8-1200mm*L Forging,hot rolling and cold rolling,Cast Black,Rough Turning,Shot Blasting,
Coil/Strip Steel Coil/Steel Strip 0.03-16.0x1200mm Cold-Rolled&Hot-Rolled Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Pipes/Tubes Seamless Pipes/Tubes,Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion,Cold Drawn,Welded Annealed,Solution and Aging,Q+T,ACID-WASHED

ISO 11 Steel Stock

Steel grade Dimension Shape Unit Quantity Delivery state Query
SkD-11 Round Bar Stock Φ30-Φ350 Round Bar Kgs 3102 Hot-Rolled+Annealed+black Enquiry
Cr12MoV 12-160(T)*310-610(W)*L Plate or Sheet Tons 12.38 Hot-Rolled+Annealed+black Enquiry
1.2601 12-160(T)*310-610(W)*L Plate or Sheet Tons 11.22 Hot-Rolled+Annealed+black Enquiry
Incoloy800 round bar Φ115*1400 Round Bar Kgs 169 Hot-Rolled+Annealed+black Enquiry
1Cr11Ni2W2MoV,961,13Cr11Ni2W2MoV Sheet Select 0 Select Enquiry