06X18Γ9H5AБ Stainless Steels

06X18Γ9H5AБ - Specification & Application

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(wt.%) of 06X18Γ9H5AБ grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.06
Si - 0.60
Mn 8.00 10.00
P - 0.020
S - 0.020
Cr 17.00 19.00
Ni 4.00 5.50
Mo - 0.30
B 0.0010 0.0030
Nb 0.15 0.25
Ce 0.01 0.03
N 0.35 0.45
Ca 0.001 0.003

06X18Γ9H5AБ - Detail

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Mechanical properties of grade 06X18Γ9H5AБ

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
422 (≥) 355 (≥) 32 34 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 232

Physical properties of grade 06X18Γ9H5AБ

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
851 (≥) 629 (≥) 33 33 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 323
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
633 696 444

Equivalent Grade

Equivalent Products

We can customize the production of 06X18Γ9H5AБ grade, contact us for the best solution.