07X17H6 Stainless Steels

07X17H6 - Specification & Application

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(wt.%) of 07X17H6 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04 0.10
Si - 0.60
Mn - 0.60
P - 0.035
S - 0.020
Cr 16.00 18.00
Ni 15.00 17.00
Mo - 0.30
Al 1.20 1.80

07X17H6 - Detail

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Mechanical properties of grade 07X17H6

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
518 (≥) 281 (≥) 14 23 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 143

Physical properties of grade 07X17H6

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
137 (≥) 641 (≥) 31 24 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 344
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
198 123 573

Equivalent Grade

Equivalent Products

We can customize the production of 07X17H6 grade, contact us for the best solution.