08X16H11M3 Stainless Steels

08X16H11M3 - Specification & Application

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(wt.%) of 08X16H11M3 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 0.80
Mn 1.00 1.70
P - 0.020
S - 0.020
Cr 15.00 17.00
Ni 10.00 12.00
Mo 2.00 2.50
Ti 0.20 0.40
V - 0.20

08X16H11M3 - Detail

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Mechanical properties of grade 08X16H11M3

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
636 (≥) 838 (≥) 21 33 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 324

Physical properties of grade 08X16H11M3

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
583 (≥) 184 (≥) 24 41 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 424
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
554 931 351

Equivalent Grade

Equivalent Products