08X20H5AΓ12MΦ Stainless Steels

08X20H5AΓ12MΦ - Specification & Application

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(wt.%) of 08X20H5AΓ12MΦ grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si 0.20 0.70
Mn 11.50 13.50
P - 0.030
S - 0.015
Cr 18.00 20.00
Ni 4.50 5.50
Mo 1.20 1.50

08X20H5AΓ12MΦ - Detail

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Mechanical properties of grade 08X20H5AΓ12MΦ

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
717 (≥) 437 (≥) 43 22 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 331

Physical properties of grade 08X20H5AΓ12MΦ

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
895 (≥) 398 (≥) 24 12 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 312
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
122 288 927

Equivalent Grade

Equivalent Products

We can customize the production of 08X20H5AΓ12MΦ grade, contact us for the best solution.
sales@specificsteel.com