0Cr15Ni25Ti2MoA1VB Stainless Steels to GB 4238 (1992)

0Cr15Ni25Ti2MoA1VB - Specification & Application

  • GB 4238 (1992) - Heat-resisting steel sheets and plates
  • GB/T 1221 (1992) - Heat-resisting steel bars

Heat-resisting steel sheets and plates

Chemical composition(wt.%) of 0Cr15Ni25Ti2MoA1VB grade: to GB 4238 (1992)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 2.00
P - 0.35
S - 0.03
Ni 24.00 27.00
Cr 13.50 16.00
Mo 1.00 1.50
Ti 1.90 2.35
Al - 0.35
B 0.001 0.010
V 0.10 0.50

0Cr15Ni25Ti2MoA1VB - Detail

0Cr15Ni25Ti2MoA1VB

Mechanical properties of grade 0Cr15Ni25Ti2MoA1VB GB 4238 (1992)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
449 (≥) 981 (≥) 13 34 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 232

Physical properties of grade 0Cr15Ni25Ti2MoA1VB GB 4238 (1992)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
154 (≥) 456 (≥) 33 13 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 132
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
436 399 175

Equivalent Grade

Equivalent Products

We can customize the production of 0Cr15Ni25Ti2MoA1VB grade, contact us for the best solution.