0Cr19Ni9N Special Alloy

Chemical composition%of the ladle analysis of grade0Cr19Ni9N

C(%)Si(%)Mn(%)P(%)S(%)Cr(%)Ni(%)N(%)
Max 0.08Max 1.00Max 2.00max 0.035Max 0.03018.00-20.007.00-10.500.10-0.25
This page is mainly introduced the 0Cr19Ni9N chemical information,mechanical properties, physical properties, mechanical properties, heat treatment, and Micro structure, etc. It also contains the use of 0Cr19Ni9N,such as it is commonly used in bars, sheet,plates, steel coils, steel pipes,forged and other materials application.

Mechanical properties of grade0Cr19Ni9N

Proof strength
Rp0.2(MPa)
Tensile strength
Rm(MPa)
Impact energy
KV(J)
Elongation at fracture
A(%)
Reduction in cross section on fracture
Z(%)
As-Heat-Treated Condition Brinell hardness(HBW)
994(≥) 557(≥) 23 14 12 Solution and Aging,Annealing,Ausaging,Q+T,etc 424

Physical properties of grade 0Cr19Ni9N

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J/kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
697(≥) 483(≥) 32 32 12 Solution and Aging,Annealing,Ausaging,Q+T,etc 222
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0)N/mm2
Creep rupture strength
(10000h)
(Rp1,0)N/mm2
968 962 768

0Cr19Ni9N Range of products

Product type Products Dimension Processes Deliver Status
Plates/Sheets Plates/Sheets 0.08-200mm(T)*W*L Forging,hot rolling and cold rolling Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Steel Bar Round Bar,Flat Bar,Square Bar Φ8-1200mm*L Forging,hot rolling and cold rolling,Cast Black,Rough Turning,Shot Blasting,
Coil/Strip Steel Coil/Steel Strip 0.03-16.0x1200mm Cold-Rolled&Hot-Rolled Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Pipes/Tubes Seamless Pipes/Tubes,Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion,Cold Drawn,Welded Annealed,Solution and Aging,Q+T,ACID-WASHED

Equivalent Grade