1.2129 Tool Die Steels

1.2129 - Specification & Application

Alloyed CrMn steel

Chemical composition(wt.%) of 1.2129 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 1.90 2.10
Si 0.15 0.30
Mn 0.80 1.10
P - 0.035
S - 0.035
Cr 1.90 2.20
Mo - -
V - -

1.2129 - Detail

Alloyed CrMn steel

Mechanical properties of grade 1.2129

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
173 (≥) 315 (≥) 41 42 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 212

Physical properties of grade 1.2129

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
487 (≥) 813 (≥) 13 44 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 313
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
686 393 849

Equivalent Grade

Equivalent Products

We can customize the production of 1.2129 grade, contact us for the best solution.
sales@specificsteel.com