Stainless steels - Part 3: Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.08 | ||
Si | - | 1.00 | ||
Mn | - | 1.00 | ||
P | - | 0.04 | ||
S | - | 0.015 | ||
Cr | 12.0 | 14.0 | ||
Ni | - | - | ||
Mo | - | - |
Stainless steels - Part 3: Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
389 (≥) | 779 (≥) | 22 | 12 | 33 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 333 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
153 (≥) | 844 (≥) | 21 | 22 | 44 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 122 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
644 | 221 | 448 |
We can customize the production of 1.4000 grade, contact us for the best solution.