1.4016 Stainless Steels to DIN 1654-5 (1989)
1.4016 - Specification & Application
- DIN 1654-5 (1989) - Cold heading and cold extruding steels; technical delivery conditions for stainless steels
- DIN 17440 (1996) - Stainless steels - Technical delivery conditions for drawn wire
- DIN 17455 (1985) - Welded circular tubes of stainless steels for general requirements; technical delivery conditions
- DIN 17456 (1985) - Seamless circular tubes of stainless steels for general requirements; technical delivery conditions
- DIN EN 10088-3 - Stainless steels - Part 3: Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes
- DIN EN 10088-4 - Stainless steels - Part 4: Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for construction purposes
- DIN EN 10088-5 - Stainless steels - Part 5: Technical delivery conditions for bars, rods, wire, sections and bright products of corrosion resisting steels for construction purposes
- DIN EN 10297-2 (2005) - Seamless circular steel tubes for mechanical and general engineering purposes - Technical delivery conditions - Part 2: Stainless steel
- DIN EN 10088-1 - Stainless steels - Part 1: List of stainless steels
- DIN EN 10088-2 - Stainless steels - Part 2: Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for general purposes
- DIN 17456 (1985) - Seamless circular tubes of stainless steels for general requirements; technical delivery conditions
- DIN 5512-3 - Materials for rail vehicles - Steels - Part 3: Stainless steel flat products; Selected standard
- DIN EN 10151 - Stainless steel strip for springs - Technical delivery conditions
- DIN EN 10250-4 - Open die steel forgings for general engineering purposes - Part 4: Stainless steels
- DIN EN 10263-5 - Steel rod, bars and steel wire for cold heading and cold extrusion - Part 5: Technical delivery conditions for stainless steels
- DIN EN 10296-2 (2005) - Welded circular steel tubes for mechanical and general engineering purposes - Technical delivery conditions - Part 2: Stainless steel
Cold heading and cold extruding steels; technical delivery conditions for stainless steels
Chemical composition(wt.%) of 1.4016 grade: to DIN 1654-5 (1989)
Elements |
Min.(≥) |
Max.(≤) |
Similar |
Remarks |
C |
- |
0.08 |
|
|
Si |
- |
1.00 |
|
|
Mn |
- |
1.00 |
|
|
P |
- |
0.040 |
|
|
S |
- |
0.015 |
|
|
Cr |
16.0 |
18.0 |
|
|
1.4016 - Detail
Cold heading and cold extruding steels; technical delivery conditions for stainless steels
Mechanical properties of grade 1.4016 DIN 1654-5 (1989)
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition |
Brinell hardness (HBW) |
133 (≥) |
339 (≥) |
44 |
42 |
13 |
Solution and Aging, Annealing, Ausaging, Q+T,etc |
342 |
Physical properties of grade 1.4016 DIN 1654-5 (1989)
Property |
Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
864 (≥) |
784 (≥) |
43 |
42 |
22 |
Solution and Aging, Annealing, Ausaging, Q+T,etc |
421 |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|
|
|
|
|
696 |
893 |
676 |
|
|
|
|
Product shapes we supply: