1.4029 Stainless Steels to BS EN 10088-1

1.4029 - Specification & Application

  • BS EN 10088-1 - Stainless steels - Part 1: List of stainless steels
  • BS EN 10088-3 - Stainless steels - Part 3: Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes

Stainless steels - Part 3: Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes

Chemical composition(wt.%) of 1.4029 grade: to BS EN 10088-1

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.25 0.32
Si - 1.00
Mn - 1.50
P - 0.04
S 0.15 0.25
Cr 12.00 13.50
Ni - -
Mo - 0.60

1.4029 - Detail

Stainless steels - Part 3: Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes

Mechanical properties of grade 1.4029 BS EN 10088-1

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
435 (≥) 948 (≥) 43 12 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 334

Physical properties of grade 1.4029 BS EN 10088-1

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
585 (≥) 652 (≥) 11 33 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 434
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
346 961 131

Equivalent Products

We can customize the production of 1.4029 grade, contact us for the best solution.