1.4542 Stainless Steels to NF EN 10088-1

1.4542 - Specification & Application

  • NF EN 10088-1 - Stainless steels - Part 1: List of stainless steels
  • NF EN 10088-2 - Stainless steels - Part 2: Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for general purposes
  • NF EN 10088-3 - Stainless steels - Part 3: Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes
  • NF EN 10088-4 - Stainless steels - Part 4: Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for construction purposes
  • NF EN 10088-5 - Stainless steels - Part 5: Technical delivery conditions for bars, rods, wire, sections and bright products of corrosion resisting steels for construction purposes
  • NF EN 10250-4 - Open die steel forgings for general engineering purposes - Part 4: Stainless steels

Open die steel forgings for general engineering purposes - Part 4: Stainless steels

Chemical composition(wt.%) of 1.4542 grade: to NF EN 10088-1

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.07
Si - 0.70
Mn - 1.50
P - 0.040
S - 0.015
Cr 15.00 17.00
Mo - 0.60
Ni 3.00 5.00
Cu 3.00 5.00
Nb 5×C 0.45

1.4542 - Detail

Open die steel forgings for general engineering purposes - Part 4: Stainless steels

Mechanical properties of grade 1.4542 NF EN 10088-1

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
919 (≥) 269 (≥) 44 23 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 424

Physical properties of grade 1.4542 NF EN 10088-1

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
479 (≥) 157 (≥) 31 13 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 123
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
774 399 373
We can customize the production of 1.4542 grade, contact us for the best solution.