1.4590 Stainless Steels to NF EN 10088-1

1.4590 - Specification & Application

  • NF EN 10088-1 - Stainless steels - Part 1: List of stainless steels
  • NF EN 10088-2 - Stainless steels - Part 2: Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for general purposes

Stainless steels - Part 2: Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for general purposes

Chemical composition(wt.%) of 1.4590 grade: to NF EN 10088-1

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.030
Si - 1.00
Mn - 1.00
P - 0.040
S - 0.015
Cr 16.00 17.50
Mo - -
Ni - -
Nb 0.35 0.55
Zr - 7×(C+N)+0.15

1.4590 - Detail

Stainless steels - Part 2: Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for general purposes

Mechanical properties of grade 1.4590 NF EN 10088-1

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
955 (≥) 345 (≥) 31 32 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 333

Physical properties of grade 1.4590 NF EN 10088-1

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
444 (≥) 269 (≥) 24 24 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 321
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
242 761 318

Equivalent Products

We can customize the production of 1.4590 grade, contact us for the best solution.