1.4605(EN) Stainless Steels to EN 10088-1 (1995)

1.4605(EN) - Specification & Application

  • EN 10088-1 (1995) - Stainless steels - Part 1: List of stainless steels
  • EN 10088-2 (1995) - Stainless steels - Part 2: Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for general purposes

Stainless steels - Part 2: Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for general purposes

Chemical composition(wt.%) of 1.4605(EN) grade: to EN 10088-1 (1995)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.030
Si - 1.00
Mn - 1.00
P - 0.040
S - 0.015
Cr 17.00 18.00
Mo - -
Ni - -
Al 1.70 2.10
Ti - 4×(C+N)+0.15-0.80

1.4605(EN) - Detail

Stainless steels - Part 2: Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for general purposes

Mechanical properties of grade 1.4605(EN) EN 10088-1 (1995)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
798 (≥) 431 (≥) 12 42 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 142

Physical properties of grade 1.4605(EN) EN 10088-1 (1995)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
457 (≥) 696 (≥) 11 23 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 131
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
742 992 573

Equivalent Products

We can customize the production of 1.4605(EN) grade, contact us for the best solution.