1.4871 Stainless Steels to NF EN 10090

1.4871 - Specification & Application

  • NF EN 10090 - Valve steels and alloys for internal combustion engines

Valve steels and alloys for internal combustion engines

Chemical composition(wt.%) of 1.4871 grade: to NF EN 10090

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.48 0.58
Si - 0.25
Mn 8.00 10.00
P - 0.045
S - 0.030
Cr 20.00 22.00
Ni 3.25 4.50
Mo - -
N 0.35 0.50

1.4871 - Detail

Valve steels and alloys for internal combustion engines

Mechanical properties of grade 1.4871 NF EN 10090

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
288 (≥) 744 (≥) 23 24 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 331

Physical properties of grade 1.4871 NF EN 10090

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
988 (≥) 978 (≥) 34 13 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 424
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
132 113 168