1.4941 Stainless Steels to NF EN 10028-7

1.4941 - Specification & Application

  • NF EN 10028-7 - Flat products made of steels for pressure purposes - Part 7: Stainless steels
  • NF EN 10088-1 - Stainless steels - Part 1: List of stainless steels
  • NF EN 10216-5 (2004) - Seamless steel tubes for pressure purposes - Technical delivery conditions - Part 5: Stainless steel tubes
  • NF EN 10222-5 - Steel forgings for pressure purposes - Part 5: Martensitic, austenitic and austenitic-ferritic stainless steels
  • NF EN 10269 - Steels and nickel alloys for fasteners with specified elevated and/or low temperature properties
  • NF EN 10302 (2002) - Creep resisting steels, nickel and cobalt alloys

Creep resisting steels, nickel and cobalt alloys

Chemical composition(wt.%) of 1.4941 grade: to NF EN 10028-7

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04 0.08
Si - 1.00
Mn - 2.00
P - 0.035
S - 0.015
Cr 17.00 19.00
Ni 9.00 12.00
Mo - -
Ti 5XC% 0.80
B 0.0015 0.0050

1.4941 - Detail

Creep resisting steels, nickel and cobalt alloys

Mechanical properties of grade 1.4941 NF EN 10028-7

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
376 (≥) 291 (≥) 22 12 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 443

Physical properties of grade 1.4941 NF EN 10028-7

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
494 (≥) 288 (≥) 41 22 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 123
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
999 362 868

Equivalent Products

We can customize the production of 1.4941 grade, contact us for the best solution.